22 March 2013 Extreme ultraviolet lithography mask etch study and overview
Banqiu Wu, Ajay Kumar, Madhavi Chandrachood, Amitabh Sabharwal
Author Affiliations +
Abstract
An overview of extreme ultraviolet lithography (EUVL) mask etch is presented and a EUVL mask etch study was carried out. Today, EUVL implementation has three critical challenges that hinder its adoption: extreme ultraviolet (EUV) source power, resist resolution-line width roughness-sensitivity, and a qualified EUVL mask. The EUVL mask defect challenges result from defects generated during blank preparation, absorber and multilayer deposition processes, as well as patterning, etching and wet clean processes. Stringent control on several performance criteria including critical dimension (CD) uniformity, etch bias, micro-loading, profile control, defect control, and high etch selectivity requirement to capping layer is required during the resist pattern duplication on the underlying absorber layer. EUVL mask absorbers comprise of mainly tantalum-based materials rather than chrome- or MoSi-based materials used in standard optical masks. Compared to the conventional chrome-based absorbers and phase shift materials, tantalum-based absorbers need high ion energy to obtain moderate etch rates. However, high ion energy may lower resist selectivity, and could introduce defects. Current EUVL mask consists of an anti-reflective layer on top of the bulk absorber. Recent studies indicate that a native oxide layer would suffice as an anti-reflective coating layer during the electron beam inspection. The absorber thickness and the material properties are optimized based on optical density targets for the mask as well as electromagnetic field effects and optics requirements of the patterning tools. EUVL mask etch processes are modified according to the structure of the absorber, its material, and thickness. However, etch product volatility is the fundamental requirement. Overlapping lithographic exposure near chip border may require etching through the multilayer, resulting in challenges in profile control and etch selectivity. Optical proximity correction is applied to further enhance the resolution. Other resolution enhancement techniques, such as phase shifting, are also in consideration for EUVL. Phase-shifting will involve partial etching of the multilayer. The trend to use shorter EUV wavelength (e.g., 6.7 nm) for enhancing resolution will use new multilayer and absorber compositions, and will require new etch process development efforts. TaBO/TaBN absorber layers (features down to 40 nm) were etched with vertical profiles, low etch CD bias, and 1.7 nm etch CD uniformity (). In the light shed application, Mo/Si multilayer etching yielded vertical profiles and high etch selectivity.
© 2013 Society of Photo-Optical Instrumentation Engineers (SPIE) 0091-3286/2013/$25.00 © 2013 SPIE
Banqiu Wu, Ajay Kumar, Madhavi Chandrachood, and Amitabh Sabharwal "Extreme ultraviolet lithography mask etch study and overview," Journal of Micro/Nanolithography, MEMS, and MOEMS 12(2), 021007 (22 March 2013). https://doi.org/10.1117/1.JMM.12.2.021007
Published: 22 March 2013
Lens.org Logo
CITATIONS
Cited by 1 scholarly publication.
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Etching

Extreme ultraviolet lithography

Photomasks

Extreme ultraviolet

Multilayers

Line width roughness

Inspection

RELATED CONTENT

Line width roughness and its control on photomask
Proceedings of SPIE (September 09 2013)
EUV sensitive Si containing hard mask (Si HM) for PTD...
Proceedings of SPIE (April 01 2013)
EUV mask development: material and process
Proceedings of SPIE (August 16 2002)
Cr absorber mask for extreme-ultraviolet lithography
Proceedings of SPIE (January 22 2001)
EUV mask fabrication with Cr absorber
Proceedings of SPIE (July 21 2000)
Inspection and repair of EUV
Proceedings of SPIE (March 11 2002)

Back to Top