30 May 2003 Identification and elimination of fluorescent surface-damage precursors on DKDP optics
Mike C. Nostrand, Samuel L. Thompson, Wigbert J. Siekhaus, Michael J. Fluss, Douglas E. Hahn, Pamela K. Whitman, Alan K. Burnham
Author Affiliations +
Abstract
Fluorescing surface defects that led to damage upon 351-nm laser exposure below 7 J/cm2 (3-ns) in DKDP optics were reported in these proceedings by this group a year ago. Subsequent laser damage experiments have correlated the density of these damage precursors to single-pont diamond finishing conditions. Every diamond-finishing schedule contains brittle-mode cutting and ductile-mode cutting in a taper-down sequence. Finishing experiments have traced the occurrence of these defects to insufficient ductile-mode removal of subsurface damage incurred during piror brittle-mode cutting. Additionally, a correlation between defect fluorescence, laser-induced damage, and defect meorphology has been established. Laser-induced damage tests also suggest a correlation between growth method and damage probability. Current experiments indicate that damage-prone defects can be minimized with the proper choice of diamond finishing conditions.
© (2003) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Mike C. Nostrand, Samuel L. Thompson, Wigbert J. Siekhaus, Michael J. Fluss, Douglas E. Hahn, Pamela K. Whitman, and Alan K. Burnham "Identification and elimination of fluorescent surface-damage precursors on DKDP optics", Proc. SPIE 4932, Laser-Induced Damage in Optical Materials: 2002 and 7th International Workshop on Laser Beam and Optics Characterization, (30 May 2003); https://doi.org/10.1117/12.472041
Lens.org Logo
CITATIONS
Cited by 2 scholarly publications.
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Crystals

Laser induced damage

Surface finishing

Diamond

Laser cutting

Laser crystals

Luminescence

Back to Top