We have developed a low density (30-670 kg/rn3), high porosity (up to 96%) foam containing lithium hydride and amorphous
beryllium hydride. This foam may be attractive as the X-ray scauering element in experiments such as the Thomson
Scattering Polarimeter as proposed for inclusion in the High Throughput X-Ray Spectroscopy Space Mission, XMM,
sponsored by the European Scientific Agency. We discuss ways to synthesize the foam, and report on physical properties
such as bulk density and porosity, electron density, uniformity of foam density, concentration of impurities, pore size
distribution, and sensitivity to moisture. The composition of the foam can be varied, but equimolar mixtures of LiH and
BeH2 give the most vigorous foaming reaction. The force needed to expand the plastic reaction mass into a foam is provided
by hydrogen and organic contaminants in the beryllium hydride that are released during the foaming reaction. Simultaneous
differential thermal analysis and thermogravimetric analysis show that the reaction is endothermic with very little mass loss.
The presence of LiBeH3 as either a reaction intermediate or final product is suggested by the fact that the most vigorous
foaming occurs with equimolar mixtures oflithium hydride and beryllium hydride.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
INSTITUTIONAL Select your institution to access the SPIE Digital Library.
PERSONAL Sign in with your SPIE account to access your personal subscriptions or to use specific features such as save to my library, sign up for alerts, save searches, etc.